I apologize for the pronunciation I write from Italy and unfortunately I do not speak English.
* For about a year I am a happy owner of a generator powermax 65 installed on the machine built by me, as a control thc use of a MP3000 dthc candcnc.
Cutting frequently steel sheet from 20 ga "0.8 mm" for the construction of pipe expansion.
I make these cuts with fine cut nozzles 40 Amp shielded, such as cutting parameters follow the manual except for the speed as 8250 mm / min in my opinion are an exaggeration
for a plasma cutting "change of direction" and then I obviated for a cutting speed of 4000 mm / min.
At the beginning when the nozzle is again present in some parts cut burr formation "photo settroe 2-3" and after a few cuts but not always with the nozzle used for a few hours is
presents an optimal situation "photo industry first."
How can I solve for a solution without burrs as in "photo area 1"?
I'm hoping for a response from the Master Jim Colt.
greetings
Tiziano
TR Exhaust
* For about a year I am a happy owner of a generator powermax 65 installed on the machine built by me, as a control thc use of a MP3000 dthc candcnc.
Cutting frequently steel sheet from 20 ga "0.8 mm" for the construction of pipe expansion.
I make these cuts with fine cut nozzles 40 Amp shielded, such as cutting parameters follow the manual except for the speed as 8250 mm / min in my opinion are an exaggeration
for a plasma cutting "change of direction" and then I obviated for a cutting speed of 4000 mm / min.
At the beginning when the nozzle is again present in some parts cut burr formation "photo settroe 2-3" and after a few cuts but not always with the nozzle used for a few hours is
presents an optimal situation "photo industry first."
How can I solve for a solution without burrs as in "photo area 1"?
I'm hoping for a response from the Master Jim Colt.
greetings
Tiziano
TR Exhaust